Hossein Besharatloo: Evaluation of PcBN using high-speed nanoindentation

Jun 29, 2020

Intrinsic hardness of each constituves phases of PcBN were evaluated. Three main hardness peaks were assessed which attributed to TiN binder, cBN particles and composite like phase. Hardness of cBN particles may vary in terms of Boron/Nitrogen ratio.