Battery Materials Technology Symposium: Operando Nanoindentation Measurement of Mechanical Properties of Battery Materials
Nov 12, 2021Dr. Kejie Zhao of Purdue University discusses in situ nanoindentation measurement to characterize local mechanical behavior in solid state batteries.